Nylon embryonic fabric heat setting finishing

Aug 06, 2019

1. Heat setting temperature: 160-180 ℃  Speed: 20m-25m/min

2. The setting temperature has great influence on the color, especially purple, pink orchid, etc. So we should pay attention to whether the color of the post-setting is the same as that of the pre-setting.

3. The shrinkage of nylon fabrics is also different in thickness.

4. It is easy to crochet nylon fabric. If there is a crochet yarn at the end of the crochet yarn, stop the machine immediately, check the machine head and tail, bellows, drums, sandpaper polishing, padding.